Technical Program
Advance Program (pdf)
| Wednesday, April 23, 2008 – Morning | |
| Welcome Introductions Peter Ried, Ried and Associates, LLC |
8:00 a.m. – 8:05 a.m. |
| THE STATE OF THE ART | |
| Die Coating and Surface Engineering for Aluminum Pressure Die Casting: State of the Art/Science John Moore, Colorado School of Mines |
8:05 a.m. – 8:35 a.m. |
| FAILURE MECHANISMS | |
| Extending Die Life Through Failure Analysis
Corwyn Berger, Bodycote Material Testing |
8:35 a.m. – 9:05 a.m. |
| Die Soldering During Die Casting of Aluminum Components Diran Apelian, Worcester Polytechnic Institute |
9:05 a.m. – 9:35 a.m. |
| AM Break |
9:35 a.m. – 9:45 a.m. |
| SOLUTIONS – Substrates | |
| Tooling Materials: Selecting the Right Substrate and the Right Preparation for Surface Coatings Patricia Miller, BÖhlerUddeholm |
9:45a.m. – 10:15 a.m. |
| Application/Success Story Don Cherry, St. Clair Die Casting |
10:15 a.m. –10:25a.m. |
Panel Discussion
|
10:25 a.m. –10:55a.m. |
| SOLUTIONS – Surface Modification | |
| Surface Modification for Die Casting Tooling – An Overview Rabi Bhattacharya, UES, Inc. |
10:55 a.m. –11:25a.m. |
| Application/Success Story Thomas Heider, Twin City Die Castings Inc. |
11:25 a.m. –11:35a.m. |
Panel Discussion
|
11:35 a.m. –12:05p.m. |
| Wednesday, April 23, 2008 – Afternoon | |
| LUNCH | |
| SOLUTIONS – Surface Coating | |
| Aluminum Die Casting: Die Coating, Lube, and Soldering Interactions Observations
David Bell, Phygen |
1:05 p.m. – 1:35 p.m. |
| Application/Success Story Randy Malterer, CONTECH |
1:35 p.m. – 1:45 p.m. |
Panel Discussion
|
|
| PM Break | 2:15 p.m. – 2:25 p.m. |
| VISION | |
| Introduction / Strategic Plan – Roadmap Peter Ried, Ried and Associates, LLC or Steve Udvardy, North American Die Casting Association |
2:25 p.m. – 2:35 p.m. |
| PANEL DISCUSSION / BRAINSTORMING | |
Compile Needs, Challenges, Opportunities
|
2:35 p.m. – 3:35 p.m. |
| CLOSING REMARKS | |
| Thank You and Next Steps Steve Udvardy, North American Die Casting Association |
3:35 p.m. – 3:45 p.m. |