    Metallography of Steels: Interpretation of Structure and the Effects of Processing

    Published: 2018
    Authors: Hubertus Colpaert

    This book is a combination of a metallographic atlas for steels and cast irons and an introductory textbook covering the fundamentals of phase transformations and heat treatment of these materials. Every important stage of processing, from casting to cold working is clearly discussed and copiously illustrated with metallographs that show the obtained structures, both desired and those achieved when deviations occur. A valuable companion even for experienced steel practitioners.

    Material Resources / Publications

    Introduction to Metallurgical Lab Practices, December 11-13, 2017

    December 11, 2017 - December 13, 2017
    Novelty, OH, 44073-0002, USA
    Instructor: Mr. John Peppler

    Basic techniques commonly used in a Metallurgical Laboratory will be taught in this class. You will become familiar with metallography by sectioning, mounting, grinding, polishing and etching samples. These samples will be examined and photomicrographs obtained by using optical microscopes equipped with digital cameras. Various Microhardness and Macrohardness equipment will be used to demonstrate the strengths and limitations of the tests. Tensile Testing and Impact Testing will be performed on standard samples. Basic principles and sample demonstration on the use of Scanning Electron Microscopy (SEM) will be covered. Hands on testing complimented by lectures on the basics of the tests will give a thorough overview of these procedures. This is the course you need if you learn by doing and could use an overview of Metallographic Lab procedures.

    Learning & Professional Development / Courses / Classroom

    Metallography for Failure Analysis, November 13 - November 16, 2017

    November 13, 2017 - November 16, 2017
    Novelty, OH, 44073-0002, USA
    Instructor: Ms. Frauke Hogue FASM

    This practical lab course focuses on metallographic techniques of failure analysis and will take you through the process of initial visual examination, fracture cleaning, documentation, and unusual metallographic sample preparation techniques and metallographic interpretation of various failure modes. You are encouraged to bring their own samples to prepare. Samples of various failure modes will also be provided.

    Learning & Professional Development / Courses / Classroom

    Advanced Metallographic Techniques, November 6-9, 2017

    November 06, 2017 - November 09, 2017
    Novelty, OH, 44073-0002, USA
    Instructor: Mr. Natalio (Nat) Saenz, FASM

    Learn basic and advanced metallographic techniques that will reveal the true microstructural characteristics of a wide range of materials.  The theory and understanding of the proper selection of abrasives, lubricants, equipment, polishing cloths/pads and a basic understanding of chemomechanical polishing will be discussed. The course covers the preparation methods of most metals and alloys, composites, hard metals, ceramics and coatings.

    Learning & Professional Development / Courses / Classroom

    Metallographic Techniques, October 30 - November 2, 2017

    October 30, 2017 - November 02, 2017
    Novelty, OH, 44073-0002, USA
    Instructor: Dr. Laura Moyer

    During this course, participants receive intensive instruction and assistance in learning the principles of metallography. Manual preparation, automatic preparation, and hands-on activities, such as preparing a variety of hard, soft, ferrous, and non-ferrous alloys, are used to demonstrate many metallographic techniques.

    Learning & Professional Development / Courses / Classroom

    Introduction to Metallurgical Lab Practices, August 28-30, 2017

    August 28, 2017 - August 30, 2017
    Novelty, OH, 44073-0002, USA
    Instructor: Mr. John Peppler

    Basic techniques commonly used in a Metallurgical Laboratory will be taught in this class. You will become familiar with metallography by sectioning, mounting, grinding, polishing and etching samples. These samples will be examined and photomicrographs obtained by using optical microscopes equipped with digital cameras. Various Microhardness and Macrohardness equipment will be used to demonstrate the strengths and limitations of the tests. Tensile Testing and Impact Testing will be performed on standard samples. Basic principles and sample demonstration on the use of Scanning Electron Microscopy (SEM) will be covered. Hands on testing complimented by lectures on the basics of the tests will give a thorough overview of these procedures. This is the course you need if you learn by doing and could use an overview of Metallographic Lab procedures.

    Learning & Professional Development / Courses / Classroom

    Compact scanning TEM microscope offers fast changes between imaging and analysis

    August 09, 2017

    Thermo Scientific, Hillsboro, Ore., introduces the Talos F200i compact scanning transmission electron microscope (S/TEM), which can be customized to meet specific imaging and analytical requirements.

    News, Magazine & Media / Industry News

    Transformations: Selected Works of G.B. Olson on Materials, Microstructure, and Design

    Published: 2017

    ASM International and The Minerals, Metals and Materials Society (TMS) have collaborated to present a collection of the selected works of Dr. Greg B. Olson in honor of his 70th birthday in 2017.

    Material Resources / Publications

    ASM Store: Material Resources

    Material resources Books With hundreds of titles in a wide variety of subject matter, the respected ASM book collection contains a wealth of materials...

    ASM Store

    Bruker launches next-gen WDXRF spectrometer for advanced quantitative analysis

    June 19, 2017

    Bruker Corp., Germany, launches its S8 Tiger Series 2, the next-generation wavelength dispersive X-ray fluorescence spectrometer, said to be the most versatile WDXRF tool available for advanced quantitative elemental analysis.

    News, Magazine & Media / Industry News