Topic: The Benefit of Hot Isostatic Pressing (HIP) and Heat Treating on Titanium Additive Manufactured (AM) Components

 

Abstract: As fabricated, AM parts do not exhibit material properties that are suited for critical aerospace, medical, energy and automotive applications. Hot Isostatic Pressing and heat treatment improve ductility and fatigue strength of metal AM components such that they can be used in these critical applications. Processing steps, static properties and dynamic fatigue properties will be presented for titanium manufactured by Electron Beam (EB) AM techniques and Direct Metal Laser Melting (DMLM) techniques.

 

Speaker: Ron Adams

 

Bio: Ron Adams holds a BS in Metallurgy from Lehigh University. Ron has spent his career in aerospace and medical metallurgical processing in manufacturing engineering, production management, and business development roles. Ron is the Director of Additive Manufacturing Business Development for Bodycote.

 

Address: Azteca in Bellevue, 150 112th Ave NE, Bellevue, WA 98004
Time: 5:30 PM Social, 6:30 PM Dinner, and 7:00 PM Presentation
Food/Cost: Light Appetizers Provided; Dinner will be ordered off a menu (typical plate ~$15)

Please send your RSVP to psasmnewsletter@gmail.com by Tuesday, November, 8th at 5pm

 

Misc:

 

We would like to thank the hospitality and educational experience we received during our September meeting at Exotic Tool Welding - pictures from the tour are included.

 

Tentative Calendar:
Dec 13 – Holiday Dinner
Jan – Joint Dinner
Feb 14 – Student Night
Mar 14 – Chemicals Related Topic
April 11 – Trustee Dinner
May 9 – Tour and/ or Picnic


Committee:
Jason Zhou [Chair]

Rebecca Ahern [Vice Chair]

Andy Ruble [Secretary]

Mary Davis [Treasurer]

 

 

 

Further Your Knowledge


MATERIAL RESOURCES

EVENTS

ISTFA 2017

Nov 05, 2017 - Nov 09, 2017

Pasadena Convention Center,
Pasedena, CA, USA