In-Situ Studies during Cyclic Loading of NiTi-Based Shape Memory Alloy Actuators

In-Situ Studies during Cyclic Loading of NiTi-Based Shape Memory Alloy Actuators

Author: P. Sedmák, P. Šittner, C. Curfs   |   Document Download   |   Product code: ZCP2014SMST101

Classified as: Shape Memory Alloys

Price: $15.00 Member Price: $12.00
ASM Points required to purchase: 12
Add To Cart

Login to view your points.  Learn more

Austenite and martensite reflections recorded in stress points denoted on the cyclic tensile stress-strain curve were analyzed for integrated intensity, lattice strain, FWHM