Making concrete green
In the construction materials technology lab, three high school students worked with Dr. Pranshoo Solanki, a professor in the Department of Technology, to research and build green concrete made of recycled waste materials and industrial by-products instead of cement, which accounts for 8% of the planet’s carbon dioxide. Students designed, manufactured, and tested their own green concrete, which can consist of fly ash, plastic fibers, glass, shredded tires, recycled aggregates, and blast furnace slag.