Price: $99 downloadable Excel file
PURCHASING OPTIONS COMING SOON!
|
Title: |
Tool Steels: Standard Designations and Compositions (ASM Alloy Center) |
|
Abstract: |
This data set contains composition and hardness data for a wide range of tool steels. It includes more than 3000 records for cold-work, hot-work, high-speed, shock-resisting, and air, oil, and water hardening tool steels along with corresponding standards and specifications. It also includes information on heat treatment methods and potential product forms. It provides information on alloy standards from the following organizations: ISO (International), CEN (Europe), ASTM and SAE (USA), and JSA (Japan). |
|
Authors / contributors: |
Data compiled by Alok Nayar. |
|
Publication date: |
2022-01-01 |
|
Sponsoring organization(s): |
ASM International |
|
Keywords: |
alloy composition, hardness, product forms, tool steels |
|
Subject tags: |
3666 (Alloy composition) 1416 (Cold work tool steel) 3889 (Hardness) 1420 (High-speed tool steel) 1423 (Hot work tool steel) 1426 (Shock resisting tool steel) 1427 (Water hardening tool steel) 2262 (Wrought product forms ) |
|
Related content: |
ASM Alloy Center Database, https://www.asminternational.org/materials-resources/online-databases/-/journal_content/56/10192/15468704/DATABASE |
|
License: |
Distributed by ASM International. All rights reserved. Use is subject to terms and conditions. |
|
Data set format: |
Structured data file saved in Microsoft Excel format, 1 MB. |