Sudosilo S.A. commissions new Nitrex installation

Nitrex, Quebec, is helping Sudosilo S.A., a leading commercial heat treatment service provider in South America, bring premier nitriding to the Argentine industrial sector with the recent commissioning of a turnkey installation. This newly operational nitriding system, represents a significant milestone as the first of its kind in Argentina, offering third-party heat treatment services to the region.

At the forefront of technological advancement, Sudosilo has embraced cutting-edge technologies to cater to various sectors, including aluminum injection, aluminum extrusion, forging, and oil applications. The integration of a NITREX system into its operations is set to establish a new benchmark for quality and precision in nitriding treatments.

The new Nitrex system adheres to CQI-9 guidelines for automotive heat treatment processes and NADCAP requirements for aerospace applications. This aligns Sudosilo with international standards, positioning the company to meet the exacting demands of both Argentine and South American markets for quality, innovation, and unparalleled service. 

The successful commissioning of the turnkey system, featuring a pit-type furnace model NX-1015 with Nitreg® controlled nitriding, Nitreg®-C controlled nitrocarburizing, and ONC® post-oxidation process technologies, was completed in November 2023. These advanced technologies ensure a uniform case depth and precise management of nitriding/nitrocarburizing/oxidation layer formation, optimizing the mechanical properties of tooling and dies. Nitreg® and Nitreg®-C contribute to enhancing surface hardness and fatigue resistance, while ONC® improves corrosion resistance. Notably, the system eliminates the need for post-finishing operations and boasts a substantial load capacity of 4400 lbs. (2000 kg). Marathon Systems Control, serving as a Nitrex representative for Latin America, played a pivotal role in expertly executing the system installation and finalizing the process validation.

https://www.nitrex.com/