Heat treatment simulation can be a tool for optimization of heat-treatment processes, but at the present this method is still limited. Therefore most HTS is based on rough simplifications of the process. Simplifications can involve the process, number of phases, transformation kinetics, continuums models instead of micro-mechanical models, etc. These simplifications also result in inaccuracies in the calculations.

For more information, click on the link below (subscription required). Then scroll to Figure 16. R Schneider; R. Mesquita; W Schützenhöfer, Distortion in Tool Steels, ASM International, 2014  https://doi.org/10.31399/asm.hb.v04d.a0005980