Advanced High-Strength Steels: Science, Technology, and Applications

Author: Mahmoud Y. Demeri   |   Hardcover   |   Product code: 05370G   |   ISBN: 978-1-62708-005-7

Classified as: Automobiles and Ground Transportation Carbon and Alloy Steels ...more

Price: $167.00 Member Price: $125.00

Advanced high-strength steels (AHSS) are experiencing rapid growth in usage in today's automotive industry and are designed to leverage steel as the optimal automotive material. This book provides a comprehensive account of the structure-property relationships in AHSS. It examines the types, microstructures and attributes of AHSS. It also reviews the current and future applications, the benefits, trends, and environmental and sustainability issues. A compelling feature of the book is its extensive use of property charts and microstructures to simplify visualization of the resulting attributes of AHSS. This book is intended to be a textbook/reference.

Mahmoud Y. Demeri holds a BSc in Chemistry/Physics, MS in Solid State Science, MS in Computer Controlled Systems, and a Ph.D. in Metallurgical Engineering. He has held positions at Ford Scientific Research Labs and FormSys, Inc. He has served as Chairman and Council Member for various committees including the USAMP/AMP Board of Directors, TMS Shaping & Forming Committee, and TMS Materials Processing & Manufacturing Division (MPMD). Dr. Demeri has authored 70 technical papers and research reports, presented 39 technical papers, organized national and international conferences, and edited four technical proceedings. He has been an active author and contributor to ASM Handbooks, published an ASTM International Standard Test, and served as NSF Panel Advisor and Adjunct Professor at Lawrence Technological University. His career has centered on testing, selection and applications of lightweight materials.

  • Publisher: ASM International
  • Published: 2013
  • Pages: 301