Marshall Space Flight Center, Huntsville, Ala., reports that Stratasys Direct Manufacturing, Minneapolis, helped build a rocket injector 15 times faster than traditional manufacturing with direct metal laser sintering.
Continue readingAlbert Kay receives ASM Distinguished Life Member award
Mr. Albert Kay, FASM, president of ASB Industries, Barberton, Ohio, is the recipient of this year’s ASM Distinguished Life Member Award.
Continue readingOerlikon sells its vacuum business to Atlas Copco
Oerlikon, Switzerland, has signed an agreement to sell its vacuum business to Atlas Copco, Sweden, to be able to focus on its strategy of growing its global surface solutions and advanced materials businesses.
Continue readingNitride coatings based on titanium and other metals protect jet engine components
Wallwork Heat Treating, England, reports that its Nitron Flight PVD-applied nitride coatings based on titanium, chromium, chromium-aluminum, and carbon/metal carbides, improve the performance of key jet engine components.
Continue readingNitride coatings based on titanium and other metals protect jet engine components
Wallwork Heat Treating, England, reports that its Nitron Flight PVD-applied nitride coatings based on titanium, chromium, chromium-aluminum, and carbon/metal carbides improve the performance of key jet engine components.
Continue readingTitanium 2016 conference to focus on world demand trends
The International Titanium Association, Northglenn, Colo., announces that the Titanium 2016 conference and exhibition will focus on the global titanium industry.
Continue readingPurdue receives grant to design strong and ductile aluminum
Purdue University, West Lafayette, Ind., announces that ASM member Prof. Xinghang Zhang has been awarded a $450,000 grant from the Dept. of Energy to investigate methods for increasing the strength of aluminum alloys.
Continue readingPresident’s Message: New TSS Board Members Announced
Congratulations to Mr. Douglas G. Puerta, Director, Aerospace Product Qualification Testing, Element Materials Technology, who has been elected to succeed me as President of TSS.
Continue readingSolar Atmospheres of California is awarded Nadcap 24-month Merit status
Solar Atmospheres of California, Fontana, announces that it has been awarded Nadcap 24-month Merit status for Heat Treating, which means that instead of having its next Nadcap audit in eighteen months, it has been granted an accreditation that lasts until July 31, 2018.
Continue readingChromium-aluminum PVD coating protects jet engine compressor vanes and seals
Wallwork Heat Treating Co., England, has developed Nitron CA, a PVD vacuum process in which a material comprised of chromium and aluminum bound with nitrogen is deposited on complex surfaces.
Continue readingNorsk Titanium to build 3D printed parts for aerospace and deliver RPD machines to New York
Norsk Titanium, Norway, recently announced agreements with Mecachrome, Thales, Boeing, and the state of New York regarding its Rapid Plasma Deposition (RPD) additive manufacturing process. Norsk says that these titanium parts have strengths equivalent to those of forgings, but at lower cost and shorter design-to-market times.
Continue readingAlcoa’s new facility to produce titanium, nickel, aluminum powders for 3D printing
Alcoa, Pittsburgh, has committed to 3D printing technology with the opening of a new powder atomization building at the Alcoa Technology Center in New Kensington, Pa.
Continue readingAMG Titanium Alloys to supply titanium aluminides for PW1100G-JM engine
AMG Advanced Metallurgical Group N.V, Amsterdam, announces that AMG Titanium Alloys and Coatings (AMG TAC) has been selected by MTU Aero Engines to provide titanium aluminides for the production of the Pratt & Whitney PurePower PW1100G-JM engine.
Continue readingCan-Eng to build a rotary furnace for heating titanium billets
Can-Eng Furnaces Intl. Ltd., Niagara Falls, Ontario, has been contracted to design, manufacture, and commission a rotary furnace system for the heating and hot working of titanium and alloy billets and preformed shapes for Weber Metals Inc. of Paramount, California.
Continue readingWallwork doubles capacity for vacuum brazing complex parts
Wallwork Heat Treating Co., England, announces that it has more than doubled its capacity for vacuum brazing complex high-performance components at its sites in Cambridge and Manchester.
Continue readingAleris to supply aluminum plate, sheet, and wing skins for Airbus aircraft
Aleris, Cleveland, Ohio, announces that it has signed a new multi-year contract with Airbus to supply aluminum plate and sheet, as well as technically advanced wing skin material, for all Airbus aircraft programs,.
Continue readingComposite with shape memory titanium alloy wire is three times more impact-resistant
Qinetiq, England, introduces an impact-resistant composite material in which highly energy-absorbent shape-memory titanium alloy wires are woven into a carbon fiber-reinforced polymer.
Continue readingAlcoa aluminum flies high on Embraer aircraft
Alcoa, Pittsburgh, announces a multiyear agreement with Embraer, Sao Paulo, in which Alcoa will supply aluminum sheet and plate for Embraer’s new E2, the second generation of its E-Jets family of commercial aircraft, a narrow-body medium-range jet airliner.
Continue readingMB Aerospace acquires Vac Aero Poland for heat treating and thermal spray
MB Aerospace, East Granby, Conn., has acquired Vac Aero (Poland) from its Canadian parent company, Vac Aero International, for its extensive range of special process capabilities, including heat treatment and vacuum brazing, vacuum carburizing, air plasma spray (APS), and high-velocity oxygen fuel (HVOF) thermal spray coatings, as well as corrosion and oxidation-resistant paint coatings.
Continue readingFacility dedicated to heat treating Mg and Al aerospace parts is Nadcap certified
Wallwork Heat Treating Co., England, announces that it has a dedicated, Nadcap-certified heat treatment facility for magnesium and aluminum components ranging from small parts to large fabrications.
Continue readingRenishaw launches additive manufacturing system and AM Solutions Centers
Renishaw, UK, introduces the new RenAM 500M additive manufacturing system, a laser-based powder bed fusion system designed specifically for the production of metal components on the factory floor.
Continue readingGKN Aerospace establishes global centers of excellence for additive manufacturing
GKN Aerospace, UK, announces that it has established global centers of excellence for additive manufacturing in the United States, Sweden, and the United Kingdom.
Continue readingOptomec awarded $4 million to develop 3D printing repair of aircraft parts
Optomec, Albuquerque, N.M., announces that the company has been awarded $4 million by AmericaMakes, the National Additive Manufacturing Innovation Institute, to develop additive manufacturing technology for the repair of aerospace metal components for the U.S. Air Force.
Continue readingBomb-sniffing locusts on the horizon
Engineers are attaching sensors to locusts so they can monitor how the insects sniff out odors.
Continue readingDelivering durable 3D printed parts for planes
Alcoa, Pittsburgh, opened a state-of-the-art, 3D printing metal powder production facility at the Alcoa Technology Center.
Continue readingIpsen delivers heat-treating solutions across the United States
Ipsen, Cherry Valley, Ill., has shipped 11 heat-treating systems to eight different states from California to Massachusetts over the past quarter, for processing parts for companies in the aerospace, energy, commercial heat treating, and coating industries.
Continue readingJuno carries nine instruments, a titanium vault, and 3D printed brackets
Developed by Lockheed Martin, Sunnyvale, Calif., the Juno spacecraft is hexagonal in shape, is 3.5 meters tall and 3.5 meters in diameter, and has a liftoff mass of about 8000 pounds.
Continue readingThree Lego aluminum astronauts travel to Jupiter on Juno
The Lego Group, Sweden, provided three 1.5-inch figurines milled out of a single block of aluminum to ride to Jupiter on the Juno spacecraft: the astronomer Galileo, and the Greek gods Juno and Jupiter.
Continue readingAtmosphere control system enables oxide-free annealing of steel, copper, brass
Linde LLC, Murray Hill, N.J., introduces the Hydroflex atmosphere control system, a universal solution for clean and bright oxide-free annealing of steel, stainless steel, copper, bronze, and brass with high reliability and repeatability.
Continue readingNew GE Aviation facilities to produce SiC fibers and ceramic matrix composites
GE Aviation, Cincinnati, has broken ground for two materials factories near Huntsville: One facility will produce SiC ceramic fiber, while the other will use SiC ceramic fiber to make tape for ceramic matrix composite components in jet engines and land-based gas turbines.
Continue reading