Learn

Technical Program

Plan today to attend the 2027 Failure Analysis Summit — the premier technical gathering that unites leading experts and professionals across the global failure analysis community. This focused event offers in-depth technical programming, educational courses and an evening networking reception designed to foster meaningful connections and collaboration. 

Thomas Ackerson

Technical Fellow
Blue Origin
Failure of an Additive Manufactured Heat Exchanger Due to Environmentally Assisted Nitridization

VIEW ABSTRACT
David Ahearn

Managing Director
Secretariat, Materials Science and Construction

Daniel P. Dennies

Consulting Metallurgical Engineer
DMS Inc.
Stress Corrosion Cracking in “Lead Free” Brass – Technical or Political Root Cause?

VIEW ABSTRACT
Satish Dixit

Director of Engineering / R&D
Plasma Technology
Failure Analysis and Prevention of Thermal Spray Coatings: Failure Mechanisms, Characterization, and Case Studies

VIEW ABSTRACT
Larry Hanke

Principal Engineer
Materials Evaluation and Engineering
Environmental Stress Cracking in Polymers – An Overview

VIEW ABSTRACT
Nikhil Kar

Senior Managing Consultant
Engineering Systems
A metallurgical analysis of a cracked Weld-Repaired High-Performance Wheel

VIEW ABSTRACT
Chris Misorski

Brunswick Fellow
Mercury Marine
Using Lab Based and Controlled Environmental Testing to Qualify Coating Systems For Demanding Consumer Products

VIEW ABSTRACT

David C. Riegner

Sr. Materials Analyst
SEA Ltd.
Testing and Assessment of Stress Corrosion Cracking in Yellow Brass: When an Environment Meets its Material

VIEW ABSTRACT
Craig Schroeder

Senior Principal Materials Engineer
EFI Global

VIEW ABSTRACT
Han Tsan

Metallurgical Engineer
Salt River Project
Closing the Loop: Integrating Metallurgical Failure Analysis into Flow Acceleration Corrosion Program Management

VIEW ABSTRACT
Amy M. Wells

Senior Polymer Scientist
Applied Technical Services (ATS)
How the Elements of Nature Influence the Failures of Plastics

VIEW ABSTRACT
Eric Weishaupt

Principal
Brush Engineering
Identifying and Distinguishing Stress Corrosion Cracking from Dezincification in Potable and Non-Potable Water Brass Components

VIEW ABSTRACT
Marc Zupan

Forencsics Engineer
APEX Applied Science and Engineering

VIEW ABSTRACT

Corporate Sponsors