Nitrocarburizing in a carrier gas to which (initially solid) urea was added led to a fast growth of the expanded austenite zone. The gaseous decomposition products of urea that develop in the furnace are highly activating, which means that activation and nitrocarburizing are achieved simultaneously.
Continue readingAlumina-forming high temperature steels offering new opportunities in heat treatment
Two novel alumina-forming steels, Kanthal APMT and Nikrothal PM 58, have corrosion resistance based on the formation of an adherent alumina layer.
Continue readingAuto parts manufacturer orders Lucifer ceramic-fiber-lined box furnace
Lucifer Furnaces Inc., Warrington, Pa., has received an order for an electric, ceramic-fiber-lined box furnace from a leading U.S. manufacturer of stamped automotive products.
Continue readingIpsen’s strategic organizational changes designed to strengthen leadership for growth
Ipsen USA, Cherry Valley, Ill., announces that several strategic changes will be made in the company’s organizational structure to strengthen its position as the leading global provider of integrated heat treatment solutions.
Continue readingSolar Manufacturing receives U.S. patent for vacuum furnace hot zone improvement
Solar Manufacturing, Souderton, Pa., announces that it has been awarded a patent for an innovation in vacuum furnace hot zone design.
Continue readingSpinning magnesium billets during extrusion enables higher ductility and lower cost
Pacific Northwest National Laboratory (PNNL), Richland, Wash., announces that its researchers have developed a method of extruding magnesium alloys that greatly improves their energy absorption by creating novel microstructures that are not possible with traditional extrusion methods.
Continue readingATI to supply isothermal forgings and nickel-base powder alloys to Pratt & Whitney
Allegheny Technologies Inc., Pittsburgh, announces that it has signed a new Long-Term Purchase Agreement (LTPA) with Pratt & Whitney, a United Technologies company, to supply isothermal forgings and nickel-base powder alloys for next-generation jet engines.
Continue readingConstellium high-strength machinable aluminum alloys for autos resist corrosion
Constellium N.V., New York, introduces HSA6, a new generation of high-strength 6000-series alloys for extrusion-based automobile crash management systems, body-in-white structural components, and battery enclosures.
Continue readingOne Minute Mentor: Residual Stress Profiles as Determined by X-Ray Diffraction
For nitrocarburizing or consecutive carburizing and nitriding, the typical stress profile is smoother than for nitriding only.
Continue readingCan-Eng mesh-belt furnace system enables both neutral hardening and carburizing
Can-Eng Furnaces Int.l, Niagara Falls, Ontario, has received an order for a mesh belt furnace system for heat treating automotive thrust races, retainer/cages, and washers.