One Minute Mentor: Induction Hardening

Spur gears, bevel gears, splined hubs, and cams are ideal components for production using powder metallurgy. Induction hardening is a method to make these parts locally hard and wear-resistant with a tougher ductile matrix.

Continue reading

Solar Atmospheres of Western PA retains SHARP accreditation

Solar Atmospheres of Western Pennsylvania, Hermitage, has been awarded three years merit status for SHARP Accreditation. The Safety and Health Achievement Recognition Program (SHARP) is designed to recognize employees and employers for their effort in establishing and maintaining all elements of an effective safety and health program.