Wisconsin Oven ships batch ovens to the manufacturing industry

Wisconsin Oven, East Troy, announced the shipment of two custom-designed Gas Fired Batch Ovens with roll-up doors. The ovens will be used to hold molded urethane wheels prior to a curing process.

The batch ovens have a maximum operating temperature of 350°F and work chamber dimensions of 9’ wide x 4’6” long x 10’6” high. The ovens are designed with electrically operated roll-up doors in the front of the oven constructed from high-temperature fabric. The door controls allow the door to open halfway or all the way by a command from a loading robot. In addition to the roll-up door on the front, a bi-parting, side-hinged, horizontal swing door is located on the rear of each oven.

These batch ovens feature a horizontal airflow arrangement, which is ideal for products arranged in multiple tiers where heated airflow cannot be directed vertically through the product. Both ovens utilize a Watlow F4T digital controller that includes a 4.3″ color touch screen, PID temperature control with adaptive tuning, and Ethernet communication capabilities for temperature control. A remote display for the flame relays is also mounted to each control panel to provide an annunciation of operation along with fault and diagnostic information.

 

https://www.wisoven.com/news/wisconsin-oven-ships-batch-ovens-manufacturing-industry

Nitrex Partners with Telfer School of Management

Nitrex, Quebec,  announced a collaboration with the Telfer School of Management, with the aim of nurturing innovation and cultivating the next generation of visionaries through the new PhD scholarship in Digital Transformation and Innovation (DTI). 

Nitrex said that this partnership echoes their commitment to driving digitalization, not only within the heat treat industry but also within academia. They added that this scholarship marks a significant leap in empowering brilliant minds to spearhead groundbreaking research, shaping the future technological landscape of industrial manufacturing.

Read further here.

Ipsen completes ISO/IEC 17025:2017 accreditation for pyrometry services

Ipsen, Cherry Valley, IL, has successfully achieved ISO/IEC 17025:2017 accreditation for calibrations, enhancing its pyrometry services. This accreditation is particularly significant for customers operating under the National Aerospace and Defense Contractors Accreditation Program (NADCAP) and Aerospace Material Specifications (AMS) 2750G.

A key update in AMS2750G, revised in 2022, mandates that calibration service providers must hold ISO/IEC 17025:2017 accreditation. This requirement encompasses temperature controller calibration, system accuracy testing (SAT), and temperature uniformity surveys (TUS).

Cavan Cardenas, Ipsen’s calibration and pyrometry coordinator, emphasized the importance of this certification: “Obtaining this lab certification reassures our customers of our capability to accurately conduct these tests. It’s crucial for us to verify the precision of our calibration equipment to provide superior support to our clients.”

Ipsen has appointed a dedicated technician for its Calibrations Lab, located at the Vacuum Technology Excellence Center in Cherry Valley, IL. This addition strengthens the company’s commitment to providing advanced calibration solutions.

Read further here.

Solar Atmospheres South Carolina facility orders 10 bar vacuum furnace

Solar Atmospheres, Greenville, SC, has announced the acquisition of a new 10-bar vacuum furnace for its Greenville, SC facility. Manufactured by Solar Manufacturing, this new horizontal vacuum furnace measures 48 inches wide, 48 inches high, and 96 inches deep. It is designed to handle loads up to 12,000 pounds and is scheduled for installation in late 2024.

The furnace will be equipped with a vacuum pumping system capable of achieving an ultimate vacuum of 1×10-6 Torr, essential for processing titanium and other high-grade alloys. It also features advanced designs for the uniform and rapid cooling of large workloads, enhancing the processing capabilities at the Greenville facility.

Steve Prout, president of Solar Atmospheres Southeast, said, “This new furnace will provide an additional option for high-pressure quenching of large components and workloads in the region. It also offers an opportunity for cost-effective thermal processing in the current economic environment.”

https://solaratm.com/solar-atmospheres-south-carolina-facility-orders-10-bar-vacuum-furnace/

One Minute Mentor: Indirectly heated fluidized-bed furnace

Most fluidized-bed furnaces are used at temperatures below 1095 °C (2000 °F), although some manufacturers have furnaces capable of treating components to temperatures through 1205 °C (2200 °F). Initially, the gas flows upward through the permeable base to agitate the particles as the pressure is gradually increased. (b) Eventually, the gas flow is sufficient to lift the small particles of refractory materials and to transform the particle movement into a violent turbulent motion.

In the early 1980s, this furnace technology seemed to be on the right track as an alternative to salt bath technology, showing similar advantages and applications but without the environmental hazard of salt compounds, waste disposal, recycling of salts, and so on. Nowadays it can be concluded that salt bath technology was partially substituted by vacuum technology, but especially for bainitic hardening (austempering processes), salt baths are still commonly used and show a slightly growing tendency, whereas fluidized beds are hardly used any more.

This temperature limitation is related to the wear and tear on the retort materials at high temperatures, which was one of the reasons for the reduced interest in this furnace type after the initial hype.

For more information, click on the link below (subscription required). Then scroll to Figure 8.

R Schneider; R. Mesquita; W Schützenhöfer, Distortion in Tool Steels, ASM International, 2014, https://doi.org/10.31399/asm.hb.v04d.a0005958

Nitrex and Linde renew their 13-year collaboration

Nitrex, Quebec, and Linde are celebrating their 13-year collaboration, which today covers Europe and North America. Nitrex said that this partnership emphasizes both companies’ positioning in terms of technology, digital, and green footprints. 

The cooperation between Linde (previously Praxair) and UPC-Marathon, a Nitrex company, began in the USA in 2010, when Linde approached UPC-Marathon to build gas panels. Eventually, the company started sending some of its clients who needed technical support in UPC’s direction.

Nitrex supplies Linde with equipment and analyses to control gas atmospheres, thanks to its competence in heat treatment and electrical fields, technical solutions, support, and world-class gas panels.

Read further here.

One Minute Mentor: Controlled Atmosphere Furnace Equipment

Heat treatment of tool steels usually requires high flexibility combined with small lots of parts. Seal quench furnaces, executed with a single heating chamber, meet this demand. Figure 5 shows a typical schematic of a single-chamber furnace, executed with a pre-chamber, which is used both for loading and unloading and also for oil quenching or gas cooling. Another execution is shown in Fig. 6, where the load is fed directly into the heating chamber (left side in the drawing). In this case the load is transported through the furnace and received after oil quenching on the right-hand side.

For more information, click on the link below (subscription required). Then scroll to Figure 5.

R Schneider; R. Mesquita; W Schützenhöfer, Distortion in Tool Steels, ASM International, 2014, https://doi.org/10.31399/asm.hb.v04d.a0005958

Processing of nano-reinforced aluminum hybrid metal matrix composites and the effect of post-heat treatment: a review

A review from the School of Engineering and Technology, India, describes the increasing demand for cutting-edge materials with a high strength-to-weight ratio and economic considerations. Lightweight materials such as aluminum (Al) and its alloys are attractive, but some properties such as low thermal stability and high wear rate limit the application of aluminum alloys (AA) to some extent. Many researchers have developed various composites to get around these restrictions and increase the performance of aluminum and its alloy. Metal matrix composites (MMCs) with nanoparticles have revealed greater mechanical and tribological properties compared with micron-sized reinforcements. This review summarizes the latest developments in this field.

Read further here. 

 

OMM: Controlled Atmosphere Furnaces

In the past, atmospheric furnaces were used quite often for heat treatment of tool steels. Due to the improved furnace technology of vacuum furnaces and their increased distribution in the market, the percentage of tools heat treated in atmospheric furnaces has fallen significantly over the last 20 to 30 years.

Furthermore, most of the atmospheric furnaces show a maximum temperature of 1100 °C (2000 °F). Therefore, the application of atmospheric furnaces is limited, with the maximum hardening temperature of the tool steel at or below 1050 °C (1925 °F).

However, for atmospheric furnaces it is essential to select an atmosphere that will protect the surface of the tool steel against the addition or the depletion of carbon during heat treatment. Therefore, it is desirable to choose one that requires no adjustment of composition to suit various steels. Ammonia-based atmospheres meet this requirement due to the ammonia dissociation at high temperatures, leading to an excess of hydrogen with the advantage of a sufficient reduction of oxidation even of high-chromium steels.

For more information, click on the link below (subscription required). Then scroll to Figure 4.

R Schneider; R. Mesquita; W Schützenhöfer, Distortion in Tool Steels, ASM International, 2014, https://doi.org/10.31399/asm.hb.v04d.a0005958

Seco/Warwick delivers Vector vacuum furnace to revolver manufacturer

Seco/Warwick, Meadville, Pa.,  received another order for the supply of a Vector vacuum furnace to a South American international manufacturer of weapons and military equipment. The furnace will process various components including barrels, reels, locks, and firearm magazines, which are expected to be reliable, of the highest quality, and perform with outstanding resistance to negative external conditions.

This will be the second solution of this type in the South American defense industry leader’s internal hardening plant. It is a single-chamber gas-cooled vacuum furnace which can be used for a variety of metal heat treatment processes and applications. This solution has been adapted to the customer’s requirements so that it is as effective as possible at delivering the precision heat treatment results required for quality weaponry.

Thanks to the large working space (900x900x1200 mm), the Vector system is designed to process quite large elements. A characteristic feature of the design is convection heating, which improves heat transfer efficiency when heating at lower temperatures, and directional cooling, which enables differentiated cooling of problematic parts in terms of shapes.

Read further here