Wisconsin Oven to ship three custom conveyor ovens to the molded-fiber industry

Wisconsin Oven, East Troy, is scheduled to ship three custom dryers to a manufacturer in the molded-fiber industry. The ovens will be used for drying thick-walled paper pulp molded fiber packaging material used in a variety of products. Molded fiber packaging is made of 100% recycled materials, making them an environmentally friendly solution for companies looking to use sustainable packaging and reduce their environmental impact.

These paper pulp drying conveyor ovens are designed with four temperature zones, and each has the sufficient capability to remove 850 pounds of water per hour from the molded pulp. The ovens feature a maximum temperature rating of 500°. The work chamber dimensions are 8’ W x 120’ L x 1’ H. A total of twelve personnel access doors with explosion relief latches are located on the sides of each unit. Each unit also has stainless steel sheet metal and structure on the wet end to reduce corrosion.

The conveyor ovens are designed with top-down and bottom-up airflow to maximize the drying rate of the paper pulp shapes. The flat wire belt continuous conveyor system uses a variable frequency drive that is adjustable from 0-3 FPM. Emergency stop buttons are located at the load and unload sections of each oven for operator safety.

Read further here. 

Medical implant hardening in a SECO/WARWICK furnace

SECO/WARWICK, Meadville, PA, announced that they will supply a Vector vacuum furnace to the Marle Group, a global manufacturer of orthopedic prostheses. The furnace on order will be used for the heat treatment of cobalt implants. Cobalt alloy hardening requires very high temperatures, and the heating process for these materials require a high puriity environment, temperature uniformity and very fast and effective cooling.

In order for cobalt alloys to be used in implantology, they must be deprived of their ferromagnetic properties. This shiny, hard metal loses this property only when it reaches a temperature higher than 1131°C. Such a high temperature makes it necessary to use a vacuum furnace in the implant production process. The furnace can not only provide such a temperature, but also guarantees its maintenance over a longer period of time. As a comparison, the temperature, above which a ferSECO/WARWICK, Meadville, PA, announced that they will supply a Vector vacuum furnace to the Marle Group, a global manufacturer of orthopedic prostheses. The furnace on order will be used for the heat treatment of cobalt implants. Cobalt alloy hardening requires very high temperatures, and the heating process for these materials require a high puriity environment, temperature uniformity and very fast and effective cooling.


Read further here.

Three from Aalberts Surface Technologies included in this years 40 under 40

Aalberts Technologies, Livonia, announced today that Angella Sell, Connor Montgomery, and Chris Pietszak are members of Heat Treat Today’s 40 Under 40 Class of 2023. The Heat Treat Today 40 Under 40 award recognizes rising leaders in the heat treat community who are giving their time, talent, and education to make the industry a great place to work.

Angella Sell, Research & Development Engineer, is a proven leader, having chaired the ASM Detroit Chapter from June 2020 to June 2021. In 2022 Angella received the ASM Detroit Chapter President’s Award for her leadership role during the challenging pandemic years. Angella is the vice-chair of the AFS Cast Iron Research Committee and will assume the role of chair in May 2024. 

Connor Montgomery, Oshkosh Plant Manager, is focused on hiring and retention practices as well on effective communications. Connor is leading major efforts to improve flow, efficiency, and throughput in the Oshkosh plant. He has introduced the use of modern lean tools such as 5S, FIFO, and Supermarkets to reduce unproductive manhours. He is actively involved in the reduction of additional waste within plant processing. 

Chris Pietszak, Quality Manager, is focsed on the implementation of and support of ISO, IATF, and Nadcap as well as CQI-9 compliance. He is a trained ISO and IATF auditor and an MTI YES Program graduate. Chris played an important role implementing the quality systems during the start-up of the Fort Smith facility. 

Read further here

One Minute Mentor: Fluidized Bed

A fluid bed results when a gas is passed upward through a bed of small solid particles at a rate fast enough to lift these particles and to create turbulence. This motion of particles, which are usually made of aluminum oxide or silica oxide, is similar to that of a fluid, which can be seen schematically in the figure.

When gas is forced upward through small holes in a supporting plate, two forces meet to raise the particles: the buoyancy of the gas and the retarding force known as aerodynamic drag. Objects to be heat treated are immersed directly into the bed of particles.

For more information, click on the link below (subscription required). Then scroll to Figure 7.

R Schneider; R. Mesquita; W Schützenhöfer, Distortion in Tool Steels, ASM International, 2014, https://doi.org/10.31399/asm.hb.v04d.a0005958

One Minute Mentor: Controlled Atmosphere Furnace Equipment

Heat treatment of tool steels usually requires high flexibility combined with small lots of parts. Seal quench furnaces, executed with a single heating chamber, meet this demand. Figure 5 shows a typical schematic of a single-chamber furnace, executed with a pre-chamber, which is used both for loading and unloading and also for oil quenching or gas cooling. Another execution is shown in Fig. 6, where the load is fed directly into the heating chamber (left side in the drawing). In this case the load is transported through the furnace and received after oil quenching on the right-hand side.

For more information, click on the link below (subscription required). Then scroll to Figure 5.

R Schneider; R. Mesquita; W Schützenhöfer, Distortion in Tool Steels, ASM International, 2014, https://doi.org/10.31399/asm.hb.v04d.a0005958

Seco/Warwick furnace to process Jet Engine components

Seco/Warwick, Meadville, PA, has developed a system to perform clean brazing processes in high vacuum as efficiently as possible, ensuring the highest protection of the treated part surfaces. The solution will be used to process jet engine components.

The German Partner carries out comprehensive repairs of technologically advanced jet engines. The company also has a research center which develops innovative repair techniques for various types of components and entire engines. The group employs several thousand qualified employees in various locations around the world and is a leader among companies repairing and providing full service MRO for jet engines. The purchase of a vertical vacuum furnace will improve production processes and significantly increase the commercial heat treater’s efficiency.

Read further here.

Quintus hot isostatic press powers new UK HIP centre

Quintus, Västerås, Sweden, has supplied a Hot Isostatic Press (HIP) to Wallwork Group’s new HIP Centre stated to open in Bury, North Manchester, England, in September 2023. The press is the model QIH 173L M URC, equipped with Quintus’ proprietary uniform rapid cooling (URC), a feature that delivers the high material uniformity required of parts designed formission-critical applications, while enabling increased productivity with optimal temperature control.

Operating at a maximum temperature of 1250°C (2282°F) and pressure of 207 MPa (30,000 psi), the technologically advanced press has a work zone measuring 800 mm (34.6 inches) in diameter and 2550 mm (100.4 inches) high, and a capacity of over 7000 kg (15,432 lbs) per cycle.

Read further here.

One Minute Mentor: Plasma Nitriding Equipment

Cold-walled (double-walled water-cooled) systems were the first generation of plasma nitriding furnaces. This technology is also a vacuum-based process but employs the principle of glow discharge to provide energy for heating and nitriding at one time. Therefore, the independent control of the temperature stability and the nitriding intensity is not possible because both processes are using the same energy source—the plasma.

The hot-wall plasma nitriding furnaces, the next generation of cold-wall ion nitriding systems, are mainly used and built now. This system ensures optimal nitriding quality by fulfilling the highest demands on temperature and nitriding process control. The big advantage of this technology is the separation of the control of the heating and the plasma nitriding parameters. The heating and temperature control of hot-wall plasma nitriding furnaces is realized by several independent heating/cooling zones, which guarantees optimal temperature homogeneity

For more information, click on the link below (subscription required). Then scroll to Figure 26.

R Schneider; R. Mesquita; H. Altena; T. Müller; P. Seemann, Processes and Furnace Equipment for Heat Treating of Tool Steels, ASM International, 2014, https://doi.org/10.31399/asm.hb.v04d.a0005958

Ipsen installs vacuum furnace at Taiwan Hodaka Technology

Ipsen, Tainan City, Taiwan, has announced the installation of a TurboTreater vacuum furnace for a customer in Southeast Asia. Established in 2002, Taiwan Hodaka Technology Co., Ltd. is an aluminum extrusion supplier, specializing in high-end aerospace aluminum alloys. 

They also produce products used in the sporting goods, consumer electronics and automotive industries. The TurboTreater boasts a work zone size of 36” (914 mm) x 36” (914 mm) x 48” (1219mm) with a weight capacity of 3000 lb (1360 kg) and normal operating temperature up to 2400 °F (1315 °C). The furnace was designed with convection heating, allowing for more uniform processing of large cross-section parts and dense loads. It is also capable of quenching at up to 12 bar positive pressure in nitrogen.

Hodaka chose Ipsen for their positive brand reputation, technical capabilities and process know-how.