One Minute Mentor: Advantages and Limitations of Heat Treatment Simulation

Heat treatment simulation can be a tool for optimization of heat-treatment processes, but at the present this method is still limited. Therefore most HTS is based on rough simplifications of the process. Simplifications can involve the process, number of phases, transformation kinetics, continuums models instead of micro-mechanical models, etc. These simplifications also result in inaccuracies in the calculations.

For more information, click on the link below (subscription required). Then scroll to Figure 16. R Schneider; R. Mesquita; W Schützenhöfer, Distortion in Tool Steels, ASM International, 2014  https://doi.org/10.31399/asm.hb.v04d.a0005980

ECM establishes new vacuum furnace entity in mexico under MEXVAC ECM name

ECM USA, Pleasant Prairie, WI, announced the official launch of its new Mexican subsidiary, ECM Mexico, operating as MEXVAC ECM, S.A. DE C.V. This development marks a significant step in expanding ECM’s presence and service capabilities within the Mexican heat treatment industry.

The ECM Mexico team is led by operations manager Juan Cruz and field service and PLC engineer José López, under the direction of Pierre-Loic Rousset and Dennis Beauchesne. The team will work closely with ECM USA to provide localized support, reflecting ECM’s long-term commitment to strengthening service infrastructure for customers across Mexico.

The new entity will serve as a dedicated supplier of vacuum furnace technologies and support services, aiming to meet growing demand in the region for high-performance thermal processing equipment.

Read more

Bodycote joins energy industries council to expand engagement with global energy sector

Bodycote, Macclesfield, UK, announced its membership with the Energy Industries Council (EIC), a leading global trade association for the energy sector. This move strengthens Bodycote’s strategic alignment with the evolving needs of the industry and reinforces its role as a provider of heat treatment and specialist thermal processing services across power generation and energy infrastructure markets.

Through its membership, Bodycote gains broader access to key industry stakeholders, enabling stronger supply chain collaboration and the pursuit of new business opportunities within the energy sector. The company serves a wide range of EIC members, fostering synergies that support innovation and operational excellence.

Bodycote’s engagement with the EIC supports its commitment to sustainability, particularly in nuclear and renewable energy markets. The partnership enhances customer access to Bodycote’s services via EIC platforms and events, further promoting solutions that improve performance, efficiency, and reliability in critical energy applications.

Read more

Pyromaitre delivers integrated heat-treating solution to GKN driveline Mexico

Pyromaitre, Lévis, Québec, announced the completion of assembly for its P-208E oven system for GKN Driveline Mexico, marking a total of four systems delivered to the client. The company developed a fully integrated solution that includes a high-speed tempering furnace, a post-treatment cooling chamber, automated loading and unloading systems, and a smoke collection unit. Each component was configured to meet the customer’s specific production requirements.

Pyromaitre specializes in resolving convective heat transfer challenges with precision and efficiency. The company focuses on driving innovation and operational performance, aiming to be a recognized leader in stress relief and tempering solutions. Its core values—integrity, innovation, customer satisfaction, and teamwork—guide its approach to delivering high-performance thermal processing systems.

Read further:

One Minute Mentor: Phase Transformations using finite-element-method (FEM) model.

Heat treatment of tool steels means several phase transformations. Every phase transformation must be described by start amount, end amount, and kinetics (change of phases depending on temperature and time). Start and end amount can be calculated with different thermodynamic software. For example, Thermocalc is well validated for tool steels. All of the aforementioned data are used as input data for a finite-element-method (FEM) model. In any case the first step of simulation models is validation, which means the comparison of experiments and mathematical simulation. The better the input data and the better the model formulation, the better are the results and the fewer loops have to be made for an appropriate model (reference model). This reference model is then used for process optimization. All these steps of model development are illustrated in the figure. 

For more information, click on the link below (subscription required). Then scroll to Figure 15. R Schneider; R. Mesquita; W Schützenhöfer, Distortion in Tool Steels, ASM International, 2014  https://doi.org/10.31399/asm.hb.v04d.a0005980