For ledeburitic tool steels (typical 8-12%-Cr cold-work tool steels and high-speed steels) the interaction of carbides with the matrix must be taken into account, especially when these carbides are strongly oriented after plastic deformation (rolling, forging) of the pre-material.
Continue readingOne Minute Mentor: Austenitizing Tool Steel
Austenitizing is the heat treatment in which the final alloy element partitioning between the austenitic matrix (which will transform to martensite) and the retained carbides occurs.
Continue readingOne Minute Mentor: Steps for Hardening of Tools as a Function of Time, Temperature, and Phase Transformation
After hot forming, tool steel usually is submitted to heat treatment processes that may be split into two major steps.
Continue readingOne Minute Mentor: Heat Treatment Applied to Tool Steels
After hot forming, tool steel usually is exposed to a heat treatment process done to produce a low-hardness condition.
Continue readingOne Minute Mentor: Sinter Hardening
Sinter hardening refers to a process in which the cooling rate in the cooling zone of the sintering furnace is fast enough to transform a significant portion of the powder metal steel matrix into martensite.
Continue readingOne Minute Mentor: Tempering Powder Metallurgy Steels
Usually, powder metallurgy steel parts having a density greater than 6.7 g/cm3 (0.242 lb/in.3) should be tempered after hardening. Recommended tempering temperatures for PM parts range from 150 to 200°C (300 to 390°F) with 175°C (350°F) being common.
Continue readingDual chamber furnace enables simultaneous hardening and tempering
Lucifer Furnaces, Warrington, Pa., announces that a Red Devil dual chamber furnace has been added to the line of analytical equipment at Laboratory Testing Inc., Philadelphia.
Continue reading