N1 Technologies Inc., Daytona Beach, Fla., reports that it has infused a borosilicate-based glass with tungsten and multilayered carbon nanotubes during the kiln melting process to produce Tungsten Glass.
Continue readingNanoSteel builds fully dense additively manufactured parts with hardness gradient
The NanoSteel Co., Providence, R.I., announces the expansion of the company’s additive manufacturing material capabilities to support metal 3D printing of complex high hardness parts.
Continue readingIntermetallic nanoparticles increase strength and ductility in alloy steel
Researchers at Pohang University of Science and Technology, South Korea, report that they have developed a lightweight steel by uniformly dispersing nanometer-sized intermetallic compounds between and within the steel’s grains.
Continue readingSematech makes progress in EUV-resist outgas testing
Sematech, Albany, N.Y., reports that promising progress has been made in qualifying outgassing specifications for extreme ultraviolet (EUV) lithography.
Continue readingHelios PFIB designed for semiconductor failure analysis and process development
FEI Corp., Hillsboro, Ore., offers the Helios PFIB for large area deprocessing to enable electrical fault isolation of advanced process ICs, and advanced failure analysis of 3D packages.
Continue readingBruker launches NanoForce nanomechanical testing system
Bruker, Billerica, Mass., introduces the NanoForce nanoindenting and nanomechanical testing system.
Continue readingTungsten-chromium-iron PM alloy has hardness of 21 GPa
The Massachusetts Institute of Technology, Cambridge, announces that researchers have developed a tungsten-chromium-iron powder metallurgy alloy that could replace depleted uranium in armor-piercing projectiles.
Continue readingLockheed Martin opens materials and thermal sciences R&D lab in Palo Alto
The Lockheed Martin Space Systems Advanced Technology Center, Palo Alto, has opened an Advanced Materials & Thermal Sciences Center for research and development.
Continue readingIHEA announces 2013-2014 board and officers
The Industrial Heating Equipment Association, Taylor Mill, Ky., recently announced its 2013-14 Board of Directors and Officers. Serving as president (shown in the photo) is Tim Lee of Maxon, a division of Honeywell. Bob Green of Bloom Engineering was named IHEA Vice-President, and B.J. Bernard of Surface Combustion was elected Treasurer. Outgoing president Mike Shay of Elster Kromschröder, assumes the role of Past President.