Magellan Aerospace receives license to manufacture Aeromet A20X aluminum castings
Magellan Aerospace, Toronto, and Aeromet Intl. Ltd., U.K., announce that Magellan’s plant in Haley, Ontario, has joined a global network of foundries licensed to cast the advanced A20X aluminum alloy, said to be the world’s strongest aluminum casting alloy.