Nucor to expand sheet mill in Kentucky from 1,600,000 to 3,000,000 tons per year
Nucor Corp., Charlotte, N.C., reports that its Board of Directors has approved an investment of $650 million to expand the production capability of Nucor Steel Gallatin, the company's flat-rolled sheet steel mill in Ghent, Kentucky.