Wallwork Heat Treating awarded Innovate UK funding to harden titanium for implants
Wallwork Cambridge, England, has been awarded funding from Innovate UK, the government-backed sponsor of breakthrough technologies, to research the medical applications of its aircraft titanium bearing hardening technology for human implants.