Seco/Warwick Partners with European Defense Sector Manufacturer
Seco/Warwick, Swiebodzin, Poland, announced its first contract with a European defense manufacturer. The company will deliver a customized single-chamber vacuum furnace equipped with advanced low-pressure carburizing technology and high-pressure gas quenching for heat treatment of steels used in firearm manufacturing. The contract represents a shift by the defense client from traditional gas carburizing to modern low-pressure carburizing, which improves quality, process predictability, and energy efficiency. The vacuum furnace approach eliminates the environmental concerns associated with