One Minute Mentor: Distortion of Corrosion-Resistant Plastic Mold Steels
Corrosion-resistant plastic mold steels are usually tempered at lower tempering temperatures than hot-work, high-alloyed cold-work, or high-speed steels. A comparison of different types of corrosion-resistant plastic mold steels with the widely used cold-work tool steel D2 with the same dimensions as in the previous example for cold-work tool steels for such heat treatment conditions can be seen in the figure and shows that all steels show a similar low dimension change in width. Regarding the