George Vander Voort of Vander Voort Consulting, presented a discussion of a tower design that ignored dynamic stresses, leading to the collapse of a radio tower.
Several specialty carburizing steel grades have been developed for specific requirements involving high-temperature performance, fracture toughness, and/or resistance to oxidation and corrosion.
Gasbarre Thermal Processing Systems, St. Marys, Pa., announces that it has formed a partnership with Humberto Bastidas from Thermal Technic Furnace Solutions in Mexico. Current and future customers can now experience the benefit of having a local Mexico resident who speaks Spanish and prides himself on providing the best possible customer service. Mr. Bastidas has many years of experience in the heat treating field and is well acquainted with the Mexican marketplace. In addition
Solar Manufacturing, Sellersville, Pa., has designed and built a vacuum furnace for processing additively manufactured parts for a large science and technology laboratory.
Engineers from Thermo-Calc Software Inc. presented a discussion at Heat Treat 2019 about procedures for extending CALPHAD models to simulate solidification and heat treatment processes.