Skip to content
Heat Treating Society
Become a Member
  • Membership
    • About Us
    • Join/Renew HTS Today!
    • Membership & Benefits
    • Society Board
    • Society Awards
    • Get Involved
      • Committees: Get Involved
      • HTS Board Nominations
  • Material Resources
    • ASM Handbooks
    • Technical Books
    • Journal of Materials Engineering and Performance
    • Heat Treater’s Guide
    • HTS Buyer’s Guide
  • Education
    • Certificate Program
    • Heat Treat Courses
  • Events
    • View All Upcoming Events
    • Heat Treat Mexico 2026
    • IMAT 2026
  • Industry News

Category: news

  1. Home
  2. news

Solar Manufacturing provides heat treating furnace to Georgia Southern University

Solar Manufacturing, Souderton, Pa., recently shipped a horizontal front-loading vacuum furnace to Georgia Southern University in Statesboro.

Continue reading

Seco Vacuum provides high-volume nitrocarburizing furnaces for auto supplier

Seco Vacuum, Meadville, Pa., announces an order for a high-volume nitrocarburizing line of furnaces serving a major carmaker through a tier-one supplier.

Continue reading

Quaker Chemical and Houghton International combine to form new industrial fluids company

Quaker Chemical Corp., Conshohocken, Pa., and Houghton International, Valley Forge, Pa., have combined to create Quaker Houghton, a global leader in industrial process fluids to the primary metals and metalworking markets.

Continue reading

Leaders of NACE International and SSPC meet to discuss potential partnership

Leaders from NACE International, Houston, and The Society for Protective Coatings, Pittsburgh, recently convened in Houston to hold further discussions about options and approaches to combining the organizations to benefit the members of both.

Continue reading

Haynes Ni-Mo-Cr-W alloy designed for low thermal expansion at 1400°F in gas turbines

Haynes International, Kokomo, Ind., announces that it has new alloy data for Haynes 244, a new Ni-Mo-Cr-W alloy developed for static parts in advanced gas turbine engines that require low thermal expansion at temperatures up to 1400°F.

Continue reading

Steel Dynamics to invest $1.9 billion to build EAF flat roll steel mill in Texas

Steel Dynamics Inc., Fort Wayne, Ind., announces that it has selected Sinton, Texas, as the site for its new state-of-the-art, electric-arc-furnace flat roll steel mill, with construction to begin in early 2020.

Continue reading

Zeiss adds ToF SIMS detection capability to Crossbeam 350/550 FIB-SEM microscopes

Zeiss, Germany, introduces advancements in analytics, tomography, sample preparation, and data integrity for its new Crossbeam 350 and 550 focused ion beam SEM microscopes, as well as new time-of-flight secondary ion mass spectrometry (ToF-SIMS) detection.

Continue reading

Buehler’s AbrasiMet M cutter features 10- to 12-inch blades, enclosed cutting arm

Buehler, Lake Bluff, Ill., introduces the AbrasiMet M Medium abrasive cutter, a compact tabletop manual saw with a powerful 5.5 hp motor designed for heavy use.

Continue reading

Höganäs launches iron-based Rockit welding powders to combat impact/abrasive wear

Höganäs AB, Sweden, launches its new Rockit 606/706 welding powders, which prolong component lifetime in tough wear environments such as the oil & gas and mining & construction industries.

Continue reading

N2 and H2 cause different white-layer phase ratios during gas nitriding of iron and steels

Researchers from Solar Atmospheres, Souderton, Pa., will discuss the influence of nitrogen and hydrogen as diluting gases during nitriding of iron and low-alloy steels at the ASM International Heat Treat 2019 conference in October.

Continue reading
  • Previous
  • 1
  • ...
  • 52
  • 53
  • 54
  • ...
  • 196
  • Next
HTS_logo_White-2
ASM World Headquarters
9639 Kinsman Road
Materials Park, OH 44073-0002
  • +1 440.671.3800
  • Member Service Center
Facebook-f X-twitter Linkedin Instagram Youtube
About ASM
  • Contact Us
  • About HTS
  • Advertise with Us
  • Technical Support
  • Legal
Membership
  • Join
  • Benefits
  • Board
  • Awards
Popular Subjects
Materials
  • Carbon and Alloy Steels
  • Stainless Steels
  • Aluminium
  • Titanium
  • Magnesium
Processing & Performance
  • Heat Treating
Who We Are

The ASM Heat Treating Society is the world’s premier membership society dedicated to the advancement of heat treating as a theoretical and applied discipline.

Affiliate Societies