IHEA announces 2013-2014 board and officers

The Industrial Heating Equipment Association, Taylor Mill, Ky., recently announced its 2013-14 Board of Directors and Officers. Serving as president (shown in the photo) is Tim Lee of Maxon, a division of Honeywell. Bob Green of Bloom Engineering was named IHEA Vice-President, and B.J. Bernard of Surface Combustion was elected Treasurer. Outgoing president Mike Shay of Elster Kromschröder, assumes the role of Past President.

Continue reading

Beralcast beryllium-aluminum alloys under consideration for F-35 Lightning II optical components

IBC Advanced Alloys Corp., Wilmington, Mass., reports that its wholly owned U.S. subsidiary, IBC Engineered Materials Corp., is working directly with Lockheed Martin to develop specific investment-cast optical components on the F-35 Lightning II aircraft to demonstrate the technical and commercial viability of Beralcast beryllium-aluminum alloys. Beralcast principal alloys are more than three times stiffer than aluminum, with 22% less weight. They can be precision cast for simple and complex three-dimensional stability. These high modulus alloys are ideal for high-performance industrial and high-tech components, as well as for a wide range of aerospace applications.

 

This collaboration enables IBC to demonstrate its expertise and industry leadership in offering rapid prototyping and advanced materials solutions to provide investment cast parts to aerospace customers with short lead times and competitive pricing.

“IBC Engineered Materials is excited to be collaborating with Lockheed Martin and believe we will demonstrate the viability of our Beralcast alloys and cast components as mechanically compliant and cost effective components for the F-35 Lightning II program,” said Ray White, President of IB-EMC. “We hope that IBC’s partnership and collaboration with Lockheed Martin will advance the potential for our engineered materials products for other aerospace industry initiatives where modulus, weight, and cost are important design criteria.”

Read the complete release.