Wall Colmonoy, Madison Heights, Mich., offers a spring session of Modern Furnace Brazing School on May 5-7 at the Aerobraze Engineered Technologies Brazing Engineering Center in Cincinnati, Ohio.
Continue readingEFD Induction offers four-cylinder crankshaft hardening machine
EFD Induction India will be displaying a crankshaft hardening machine model at the IMTEX show to be held January 22-28 in Bangalore.
Continue readingJ.L. Becker installs car bottom furnace with duplicate combustion and control systems
J.L. Becker, a Gasbarre Furnace Group Company, Plymouth, Mich., has installed two similar furnace systems for a domestic alloy manufacturer.
Continue readingNanovea automated indentation technology eliminates user error
Nanovea, Irvine, Calif., announces the M3 hardness tester with automated indentation technology.
Continue readingHi-Tek Manufacturing receives Nadcap accreditation for heat treating and more
Hi-Tek Manufacturing, Mason, Ohio, which serves the gas turbine industry, announces that it has received Nadcap accreditation for heat treating and for brazing, hardness testing for heat treating, and pyrometry capabilities.
Continue readingSolar Atmospheres heat treats titanium manifold for Orion spacecraft
Solar Atmospheres of Western Pennsylvania, Hermitage, Pa., announces that it vacuum heat-treated the titanium manifold in the Launch Abort System of the NASA Orion spacecraft launched in December.
Continue readingAjax Tocco temper ovens heat treat automotive constant-velocity joints
Ajax Tocco Magnethermic Corp., Warren, Ohio, has supplied three temper ovens to a major automotive parts manufacturer in Mexico for the tempering of constant-velocity joints.
Continue readingVac Aero high-pressure quench vacuum furnace has high heating rates, tight uniformity
Vac Aero, Burlington, Ontario, has sold a VAH4848 HV-6 high-pressure quench vacuum furnace to a manufacturer and integrator of high performance aerospace systems and components.
Continue readingLucifer Furnaces offers furnace with separate hardening and tempering chambers
Lucifer Furnaces, Warrington, Pa., offers Red Devil Model RD8-KHE24, a space saving dual chamber unit with working dimensions of 12 x 14 x 24 inches in both upper and lower chambers.
Continue readingH.C. Starck and Rapid Prototyping and Manufacturing partner to develop 3D products
H.C. Starck, Newton, Mass., and Rapid Prototype and Manufacturing (RP+M), Avon Lake, Ohio, announce an agreement to develop advanced, innovative products using the latest 3D printing and technology metal manufacturing.
Continue reading