Lehigh University, Pa., announces that its researchers have developed plasma-enhanced atomic layer deposited titanium and vanadium nitrides that are said to be harder than commercial coatings “by orders of magnitude.”
Continue readingEuropean team produces 3D printed titanium pressure vessel for space exploration
A European aerospace production team comprising Thales Alenia Space, Cranfield University, and Glenalmond Technologies announces the completion of the first full-scale prototype of an additively manufactured titanium pressure vessel to be used in future manned missions for space exploration.
Continue readingTungsten-based alloy withstands radiation in nuclear fusion devices without damage
Los Alamos National Laboratory, New Mexico, announces that its scientists have developed a tungsten-based alloy that can withstand unprecedented amounts of radiation without damage.
Continue readingAsylum Research Jupiter AFM provides 200-mm sample access and higher resolution
Oxford Instruments Asylum Research, Santa Barbara, Calif., announces the new Jupiter XR Atomic Force Microscope, the first and only large-sample AFM to offer both high-speed imaging and extended range in a single scanner.
Continue readingMineral and organic acids extract rare earth elements from phosphate rock waste
Researchers from Rutgers University-New Brunswick, N.J., and members of the Critical Materials Institute in Ames, Iowa, announce that they have found a possible new source of rare earth elements in phosphate rock waste, and have developed an environmentally friendly way to extract the elements.
Continue readingKermetico makes specialized HVAF systems for a wide variety of powders and substrates
Kermetico, Benicia, Calif., makes specialized HVAF systems to spray metal coatings and alloyed powder compositions onto uncommon substrates such as acme threads, thin walls, and temperature-sensitive materials.
Continue readingSpray Tips: Cold spray particle velocity and temperature
The diagram compares the particle velocity and gas temperature ranges of cold spray and other thermal spray processes: In the cold spray process, the gas and particle temperatures are much lower and the gas and particle velocity are much higher than in other thermal spray processes.
Continue readingHow cold spray technology improves the electrical and erosion properties of polymers
Metallization of polymers is an attractive way of improving their electrical and erosion properties, but it is still challenging to achieve a dense metal coating on polymer surfaces by thermal spray processes, due to excessive surface erosion during processing.
Continue readingSuper-fast high-energy X-rays reveal defects in 3D printed products as they are being built
Engineers from Carnegie Mellon University and Argonne National Laboratory report that they have discovered defects in the products of the Laser Powder Bed Fusion (LPBF) process by taking videos of the products with super-fast high-energy x-rays as they are being built.
Continue readingOne Minute Mentor: Austenitizing ductile cast iron
The usual objective of austenitizing is to produce an austenitic matrix with as uniform a carbon content as possible prior to thermal processing. The graph shows the 2% silicon section of the Fe-C-Si phase diagram.