Heat Treatment with a Turbulent Twist

Furnace atmosphere circulation is at the heart of the heat treatment process: without thorough circulation of gases, heat treatment processes cannot achieve consistent results in terms of surface quality and mechanical properties.

One Minute Mentor: Crevice Corrosion Testing

In crevice corrosion testing, treated 316 stainless steel compares favorably with alloy 625, as shown in the figure with three images. This figure shows three specimens at the end of a weeklong crevice corrosion test in natural seawater, at room temperature, under an applied potential of 300 mV.