Meridian Lightweight Technologies, Plymouth, Mich., announces that Birmingham City University, England, has signed an exclusive partnership with Meridian, the world’s largest producer of magnesium components, to showcase magnesium as a viable alternative for luxury car makers and the aerospace industry.
3D optical microscope provides high combined lateral and vertical resolution
Bruker Corp., Billerica, Mass., reports that its Contour Elite 3D optical microscopes provide the high sensitivity and stability necessary for precision 3D surface measurements in applications and environments that are challenging for other metrology systems, such as R&D applications within the semiconductor and MEMS markets.
Ultralight auto door made of aluminum, polymers, and electronic latch system
Magna International Inc., Troy, Mich., in cooperation with the U.S. Department of Energy and partners FCA US and Grupo Antolin, announces that the team has developed an ultralight auto door that achieves the project objective of 42.5% mass savings over an average current production door.
One Minute Mentor: Radio-Frequency Plasma
Glow-discharge plasma nitriding is carried out in nitrogen-hydrogen atmospheres at pressures in the range of 100 to 1000. At pressures below 10 Pa, the glow-discharge technique is not used, but plasma can still be generated by radio-frequency (RF) excitation, microwave energy, or electrons produced by a heated filament.
NIST awards $12 million to MEP centers in 11 states to support manufacturers
The National Institute of Standards and Technology, Gaithersburg, Md., announces that its Hollings Manufacturing Extension Partnership (MEP) program has awarded a total of nearly $12 million in first-year funding to 11 organizations that will operate MEP centers in Delaware, Hawaii, Iowa, Kansas, Maine, Mississippi, Nevada, New Mexico, North Dakota, South Carolina, and Wyoming.