Bodycote, Macclesfield, England, announces that it has acquired Nitrex Metal Technologies, which specializes in precision gas nitriding and ferritic nitrocarburizing in both batch and continuous processes.
Chromium Nitride in Duplex Stainless Steels
Because of the use of nitrogen as an alloying element in these stainless steels, chromium nitrides (CrN) may be present on ?/? grain boundaries, on ?/? boundaries, and within the ? grains. If formed in large quantities and under conditions in which the chromium-depleted areas do not have time to repair themselves during annealing, the presence of CrN may adversely affect corrosion resistance.
Director of Canadian thermal spray research center elected Fellow of Royal Society of Canada
The University of Toronto announces that Distinguished Professor in Plasma Engineering Javad Mostaghimi has been elected a Fellow of the Royal Society of Canada for his research on simulating the dynamics of droplet impact and solidification in thermal spray coating processes.
Strong scandium-aluminum-magnesium powder-metal alloy designed for 3D printing
Airbus Group APWorks GmbH, Germany, in cooperation with Airbus Group R&D, has developed Scalmalloy, a high-performance scandium-aluminum magnesium powder metal alloy designed for additive manufacturing of high-strength aerospace structures.
Sandvik super-duplex stainless steel selected for prototype boat
2016-09-07 17:54]]> Sandvik Materials Technology, Sweden, announces that its Sandvik SAF 2507 high-strength super-duplex stainless steel has been selected for Project P16 Prototype, an innovative 56-foot prototype boat being built by Swedish Steel Yacht AB. The aim of the project is to evaluate an entirely new technology for constructing more efficient, stronger, and maintenance-free vessels. […]