Instron celebrates 70 years in business

Instron, Norwood, Mass., celebrated its 70th anniversary on March 15, 2016, marking continued success in providing customers with the highest quality products, expert support, and world-class service.

Harper issued patent for heat treatment of carbon fibers

Harper International, Buffalo, N.Y., announces that it has received a patent for its advanced carbon fiber oxidation oven technology that enables changing the airflow direction within the oven to produce down-flow and center-to-end flow throughout the process.