Praxair Inc., Danbury, Conn., has signed an agreement with Atmosphere Engineering that will allow customers to access Praxair’s industrial gases, application technologies, and supply systems, as well as Atmosphere Engineering’s furnace control systems and sensors.
Fireworks at Heat Treat Social Event Causes an International Stir
MATERIALS PARK, OH – October 26, 2015 – Last week at Heat Treat 2015, the ASM Heat Treating Society rolled out their new social event, “The Heat Is On”, which included a fireworks display that delighted guests and locals alike.
Isothermal Transformation Diagram for Tool Steels
The graph shows the isothermal transformation diagram for the steel AISI 1075/DIN EN C75. Cooling curves show three process cycles for molten metal quenching in the time-temperature-transformation plots.
One Minute Mentor: Isothermal Transformation Diagram for Tool Steels
The graph shows the isothermal transformation diagram for the steel AISI 1075/DIN EN C75. Cooling curves show three process cycles for molten metal quenching in the time-temperature-transformation plots.
Bodycote expands hot isostatic pressing capacity
Bodycote, England, is expanding its high pressure Hot Isostatic Pressing (HIP) capability with the addition of a new mid-range vessel to increase its volume capacity.