Can-Eng Furnaces International Ltd., Niagara Falls, Ontario, has been contracted to design, manufacture, and commission an automated system for the heat treatment of thin-walled high pressure diecast aluminum automotive structural components.
Spray Tips: Temperature, Dwell Time, and Velocity in the Thermal Spray Jet
Temperature and velocity vary considerably within the jet, because of several factors. The most significant of these is the difference in temperature between the hot core of the jet and its relatively cold surrounding environment.
Message from the President: Thermal Spray of Suspensions & Solutions Symposium (TS4)
For the first time in North America, a special symposium dedicated to this emerging thermal spray process will bring together scientists and engineers from academia, national laboratories, and industry for a two-day information-exchange event.
NanoSteel BLDRmetal powders for binder jet 3D printing make parts that resist wear
NanoSteel, Providence, R.I., introduces its first powders designed for the binder jet 3D printing of parts having three times the wear and impact resistance of an equivalently infiltrated 420 stainless steel.
Zircotec coatings protect Bloodhound land-speed record car from high temperatures
Zircotec Ltd., England, has provided its ThermoHold ceramic coating for the exhaust system and a zirconia-based coating for the composite front structure of the British Bloodhound, a car being designed to reach 1000 mph and break the land speed record.