One Minute Mentor: Tempering Powder Metallurgy Steels
Usually, powder metallurgy steel parts having a density greater than 6.7 g/cm3 (0.242 lb/in.3) should be tempered after hardening. Recommended tempering temperatures for PM parts range from 150 to 200°C (300 to 390°F) with 175°C (350°F) being common.
Expo sells out for Heat Treat
The ASM Heat Treating Society announced that the exposition for Heat Treat 2015 has sold out for the second time in a row. Hundreds of heat treating companies and gear manufacturers will be displaying their latest and greatest products and services next month at the 28th annual ASM Heat Treating Society Conference and Exposition in […]
Proceq Equotip 550 portable instrument for hardness testing diagnoses roll imperfections
Proceq, Switzerland, introduces the Equotip 550 Leeb U roll hardness tester, designed for testing small, midsize, and large paper rolls, as well as thin-film, foil, and coated rolls.
MTS introduces its most energy-efficient hydraulic power unit
MTS Systems Corp., Eden Prairie, Minn., announces the release of the new MTS SilentFlo 515 hydraulic power unit.