LPW Technology Inc., Pittsburgh, and Metalysis, U.K., have formed a collaboration with the goal of developing an alternative supply chain for clean, spherical tantalum and tungsten powders for critical applications.
Solar Atmospheres Southeast opens in South Carolina
Solar Atmospheres, Souderton, Pa., announces that its new plant in Greenville, S.C., has officially opened its doors for business, bringing the first furnace online the first week of May.
Lei Zhang wins 2015 HTS/Bodycote Best Paper in Heat Treating Award
Lei Zhang, a Ph.D. student in materials science engineering at Worcester Polytechnic Institute, is the winner of the 2015 HTS/Bodycote Best Paper in Heat Treating Award.
Roger Jones receives 2015 George Bodeen Heat Treating Achievement Award
Roger A. Jones, corporate president of Solar Atmospheres Inc., Souderton, Pa., is the recipient of the 2015 George H. Bodeen Heat Treating Achievement Award.
Outokumpu now categorizes its stainless steels by properties instead of chemistry
Outokumpu Oy, Finland, has developed a way to categorize its wide range of stainless steel products by arranging them according to strength, hardness, machinability, heat resistance, and corrosion resistance.