Stratasys, Minneapolis, announces that triple-jetting technology is now available cross-platform, providing up to 20% faster fused-deposition-modeling production.
Precious metal additive manufacturing system for jewelry enables lower cost
Cooksongold, England, and EOS GmbH, Sweden, have launched the Precious M 080 Direct Metal Laser Sintering (DMLS) system.
Optomec announces record orders for 3D printers
Optomec, Albuquerque, N.M., announces that its order bookings have more than doubled through the first three quarters of 2014.
Canadian consortium to promote development of additive manufacturing
Canadian Manufacturers & Exporters, Ottawa, Canada’s largest trade and industry association, has announced the launch of Canada Makes, a national network created to promote additive manufacturing.
ß-TCP added to hydroxyapatite implant coatings reduces risk of infection
Aalto University, Finland, reports that its researchers and partner manufacturers have proven that by adding a certain amount of beta-tricalcium phosphate (ß-TCP) to hydroxyapatite coatings on biomedical implants, integration is improved and the likelihood of infection is reduced.