Engineers from Tecnar Automation and Concordia University, both of Quebec, presented “Accuraspray 4.0 to Characterize In-flight Particles in the SPS Process.”
Leaders of NACE International and SSPC meet to discuss potential partnership
Spray Tips: Wire and Rod Feeders for Thermal Spray
Materials that can be thermally sprayed include polymers, metals, metal alloys, intermetallics, ceramics, and composites. The feedstock material can take the form of wire, rod, powder, or, with emerging solution spraying, liquid and complex gases. This leads to two basic types of feed systems: one that feeds wires or rods, and another that feeds particulates.
Haynes Ni-Mo-Cr-W alloy designed for low thermal expansion at 1400°F in gas turbines
Haynes International, Kokomo, Ind., announces that it has new alloy data for Haynes 244, a new Ni-Mo-Cr-W alloy developed for static parts in advanced gas turbine engines that require low thermal expansion at temperatures up to 1400°F.
Steel Dynamics to invest $1.9 billion to build EAF flat roll steel mill in Texas
Steel Dynamics Inc., Fort Wayne, Ind., announces that it has selected Sinton, Texas, as the site for its new state-of-the-art, electric-arc-furnace flat roll steel mill, with construction to begin in early 2020.