Big River Steel, Osceola, Ark. announces a major expansion of its scrap recycling and steel production facility that will double its hot-rolled steel production capacity to 3.3 million tons annually.
U.S. manufacturer of electronic components orders Despatch ovens worth $3 million
Despatch Industries, Minneapolis, announces that a major U.S. manufacturer of electronic components has placed an order worth over $3 million for Despatch PND inert atmosphere ovens.
New CFRC Info and Performance in Oil Quenching
For decades, successful manufacturers of precision parts used heat treating fixtures made of various alloy materials, but over time, these alloys would become distorted and embrittled.
Effect of Annealing Time and Temperature on Aged Properties
The graph shows the influence of solution-annealing temperature on the aged tensile properties of consumable vacuum-melted 18Ni Marage 250 steel.
Ipsen ships 18 furnaces in Q2, including 210,000-pound capacity vacuum furnace
Ipsen USA, Cherry Valley, Ill., announces that shipments in the second quarter included 18 furnaces to companies in six states in the United States and two companies overseas.