Electromagnetic induction has provided reliable, predictable, and cost-effective heat treatment results for decades.
Solar Atmospheres thermally treats first FAA-certified titanium AM aviation structural parts
Solar Atmospheres, Hermitage, Pa., has successfully processed the first FAA-Certified structural additively manufactured Ti-6Al-4V parts.
Ipsen granted U.S. patent for advanced loader design for heat treating systems
Ipsen, Cherry Valley, Ill., was recently awarded U.S. Patent No. 9,719,149 B2 for the development of a new load transport mechanism that can move a load within a multi-station heat-treating system.
Arconic to invest $137 million in new horizontal furnace to heat treat large aluminum plate
Arconic Inc., New York, plans to invest $137 million to install a new horizontal heat treat furnace at its Davenport Works facility in Iowa to heat treat longer and thicker plate than ever before.
SupremEX aluminum composite specification approved for aerospace applications
Materion Corp., Mayfield Heights, Ohio, announces that the Society of Automotive Engineers – Aerospace Material specification Nonferrous Alloys Committee (SAE-AMS) has approved specification of AMS4368 for Materion’s SupremEX 640XA aluminum composite.