One Minute Mentor: Nitriding Potential
The nitriding potential controls the amount of nitrogen in the metal. The graph shows the atomic concentration of nitrogen as a function of nitriding potential (Kn) and depth.
CompuCore expands controls retrofit options for vacuum heat treating systems
Ipsen, Cherry Valley, Ill., introduces CompuCore, a competitively priced option for controls retrofits available for installation on most brands of vacuum heat-treating systems.
Solar Atmospheres adds new furnace with 5×10-6 Torr vacuum and all-moly hot zone
Solar Atmospheres of Western Pennsylvania, Hermitage, recently added a state-of-the-art vacuum furnace with an all-molybdenum hot zone having dimensions 24 x 24 x 36 inches.
Heavy Carbon president awarded patent for Endocarb carburizing system
The Heavy Carbon Company, Pittsford, Mich., announces that its president, George Barbour, has been awarded a patent for “A method of carburizing which allows a carburizing process in a furnace at high temperatures in a protective atmosphere.”