AK Steel, Westchester, Ohio, launches its Nexmet 440EX high-strength steel that provides greater ductility, strength, and formability for automotive applications.
Aleris Aluminum to be acquired by Chinese aluminum extrusion company
Aleris Corp., Cleveland, Oho, a global aluminum rolled products producer, announces that it has entered into a definitive agreement to be acquired by Zhongwang USA LLC, a Chinese company.
Precipitation of Intermetallics in Stainless Steels
The exposure of duplex stainless steels to temperatures in the range of 1100 to 1850°F can result in the formation of undesirable intermetallic compounds such as ? and ? phases.
One Minute Mentor: Precipitation of Intermetallics in Stainless Steels
The exposure of duplex stainless steels to temperatures in the range of 1100 to 1850°F can result in the formation of undesirable intermetallic compounds such as σ and χ phases.
CERN heat treating furnace to process niobium-tin superconducting magnets
The European Organization for Nuclear Research (CERN), Geneva, announces that it has received a 105-foot-long furnace for the heat treatment of niobium-tin (Nb3Sn) superconducting coils that will be installed in the Future Circular Collider.