Epner Technology, Brooklyn, N.Y., was chosen to use its Laser Gold technology to electroplate gold onto the cast bronze Oscar statuettes this year.
One Minute Mentor: Hardness Gradients in Nitrided High-Speed Tool Steel
The graph shows the effect of bath conditions and immersion time on hardness gradients in Type T1 high-speed tool steel.
NIST ultrasound method detects cracks in capacitors
The National Institute of Standards and Technology, Gaithersburg, Md., and collaborators have demonstrated a nondestructive acoustic method for detecting cracks in ceramic capacitors before they go bad.
3D-printed titanium hip implant features fully porous acetabular cup
Smith & Nephew, Andover, Mass., introduces its first 3D-printed titanium hip implant, the new Redapt revision acetabular fully porous cup with Conceloc technology.
Bonnell Aluminum to invest $18 million in extrusion line for auto structures
Bonnell Aluminum, Newnan, Ga., announces it will invest approximately $18 million over the next year to fund an expansion project that will include the purchase of a new state-of-the-art aluminum extrusion line at its Aacoa facility in Niles, Michigan.