Constellium, Paris, announced that they are participating in the U.S. Environmental Protection Agency (EPA) Energy Star program as an Industrial Partner. The Energy Star program is a voluntary initiative that helps businesses protect the environment by promoting energy-efficient products, homes, buildings and manufacturing plants, as well as save on energy costs. As an Industrial Partner, […]
Search
Home Search FILTERS APPLIED CURRENT SEARCH Clear all REFINE RESULTS Keyword(s) New Search Search Within results Subject Resource Type
One Minute Mentor: Salt Bath Nitrocarburizing
Salt bath nitrocarburizing is usually performed at temperatures between 560 and 580 °C (1040 to 1075 °F) in cyanate- and carbonate-containing salts with traces of cyanides and furnaces similar to those used for the nitrocarburizing of mechanical compounds. These conditions fit well with the usual tempering temperatures of hot-work tool steels, which form the main […]
Can-Eng Furnaces contracted for continuous quench and temper furnace system
Can-Eng Furnaces International Ltd., Niagara, Ontario, was recently contracted to engineer and commission a continuous quench and temper furnace system for a North American producer of mining, construction, and materials handling products. The purchase of this equipment is part of a larger plant expansion and initiative to bring foreign outsourced manufacturing in house. This move […]
Ipsen installs vacuum furnace at Taiwan Hodaka Technology
Ipsen, Tainan City, Taiwan, has announced the installation of a TurboTreater vacuum furnace for a customer in Southeast Asia. Established in 2002, Taiwan Hodaka Technology Co., Ltd. is an aluminum extrusion supplier, specializing in high-end aerospace aluminum alloys. They also produce products used in the sporting goods, consumer electronics and automotive industries. The TurboTreater boasts […]