For the first time in North America, a special symposium dedicated to this emerging thermal spray process will bring together scientists and engineers from academia, national laboratories, and industry for a two-day information-exchange event.
NanoSteel BLDRmetal powders for binder jet 3D printing make parts that resist wear
NanoSteel, Providence, R.I., introduces its first powders designed for the binder jet 3D printing of parts having three times the wear and impact resistance of an equivalently infiltrated 420 stainless steel.
Zircotec coatings protect Bloodhound land-speed record car from high temperatures
Zircotec Ltd., England, has provided its ThermoHold ceramic coating for the exhaust system and a zirconia-based coating for the composite front structure of the British Bloodhound, a car being designed to reach 1000 mph and break the land speed record.
RIT chosen to lead university-industry consortium to advance additive manufacturing
Rochester Institute of Technology, Rochester, N.Y., announces that it has been chosen to lead a consortium of universities and corporations in establishing a New York State Center for advanced technology in additive manufacturing and functional printing.
Market analysis predicts thermal spray coatings market to reach $12 billion by 2022
Grand View Research Inc., San Francisco, has published a thermal spray coating market analysis that predicts the market is expected to reach $12.29 billion by the year 2022.