Engineers at Ipsen, Cherry Valley, Ill., explain that by properly tuning the proportional-integral-derivative (PID) settings in the furnace controller, users can ensure that the furnace reaches and maintains the correct setpoint temperature.
Flexible polymer electrodes printed with improved electrical properties
The Technical University of Munich (TUM) announces that its researchers have printed razor-thin polymer electrodes with improved electrical properties.
ATI achieves PQ titanium product and process qualification
Allegheny Technologies Inc., Pittsburgh, has achieved qualification for its premium-titanium products for jet engine rotating parts made of premium-quality titanium sponge from ATI’s facility in Rowley, Utah.
AFC-Holcroft supplies two universal batch quench furnaces to Paulo Products
AFC-Holcroft, Wixom, Mich., has supplied two new Universal Batch Quench furnaces to Paulo Products Co., a commercial heat treater headquartered in St. Louis, to be installed at its Kansas City Division.
Carpenter agrees to supply powder metallurgy superalloys to Pratt & Whitney
Carpenter Technology Corp., Wyomissing, Pa., reports that operations will begin soon at its new superalloy powder facility in Alabama as part of a multi-level agreement with United Technologies Corporation’s Pratt & Whitney Division.