AK Steel, West Chester, Ohio, announces that it will invest $36 million build a new world-class Research and Innovation Center in Middletown, Ohio.
American Specialty Alloys to build $2.4 billion aluminum mill complex
American Specialty Alloys Inc., Baton Rouge, La., plans to develop a $2.4 billion mill and campus in Central Louisiana to provide aluminum for the automotive and aerospace industries.
Intermetallic nanoparticles increase strength and ductility in alloy steel
Researchers at Pohang University of Science and Technology, South Korea, report that they have developed a lightweight steel by uniformly dispersing nanometer-sized intermetallic compounds between and within the steel’s grains.
Solar Atmospheres wins renewal of Sikorsky approved-supplier status
Solar Atmospheres Inc., Souderton, Pa., has received renewed approved-supplier status from Sikorsky Aircraft Corp., with a two-year certification.
Carbon control during sintering improves quality of MIM parts
Linde North America Inc., Murray Hill, N.J., and Megamet Solid Metals, Earth City, Mo., a custom metal-injection molding company, have shown that the quality of metal-injection-molded parts could be significantly enhanced by following Linde’s advanced Sinterflex atmosphere control system.