TimkenSteel Corp., Canton, Ohio, announces plans to invest $40 million to build an additional continuous heat-treating facility in the United States.
Phased-array wheel probe designed for ultrasonic inspection without immersion
Olympus America, Center Valley, Pa., introduces the RollerForm, a new phased-array wheel probe designed for ultrasonic inspection of composites and other smooth-surfaced materials.
Sciaky’s electron beam additive manufacturing systems now available for purchase
Sciaky Inc., a subsidiary of Phillips Service Industries, Chicago, will now offer its electron beam additive manufacturing (EBAM) systems for purchase, with accelerated delivery opportunities available as early as Sept. 1.
ThyssenKrupp Steel Europe invests $121 million to modernize Duisburg continuous caster
ThyssenKrupp Steel Europe, Germany, is investing $121 million to modernize continuous caster 1 in Duisburg-Beeckerwerth to improve slab quality and widen the product range.
AK Steel acquires Severstal’s Dearborn steelmaking assets
AK Steel, West Chester, Ohio, has signed an agreement to acquire Severstal North America’s integrated steelmaking assets located in Dearborn, Mich., for $700 million in cash.