Better catalysts from super-fast heating

HighT-Tech, Md., has won The Spinoff Prize 2021 for developing a technique to make alloys that could improve catalysts or be used to build better batteries. The method enables the startup to fine-tune the catalytic activity of the materials and discover new and potentially more efficient catalysts.

Solar Atmospheres vacuum heat treats longest nickel alloy tubes ever

Solar Atmospheres of Western Pennsylvania, Hermitage, Pa., successfully vacuum heat treated the largest and longest load of nickel alloy tubing ever in a commercial vacuum furnace. They were able to preserve the brightness and cleanliness of a 45-foot-long seamless tubing while meeting extremely stringent mechanical properties.

One Minute Mentor: Effect of porosity on the heat treatment of powder metallurgy steels

Porosity has the greatest single effect on the response of PM Steels to heat treatment compared with conventional steels. The majority of parts have a porosity between 5 and 15 vol%, far more than is found in a typical casting. Every mechanism in press and sinter is subject to diminishing returns; i.e., compact density has a decreasing dependence on compaction pressure, as does sintering and homogenization.