Solar Atmospheres, Greenville, SC, announced that its facility has received approval from Parker Aerospace, further expanding the company’s capabilities to meet aerospace industry demands. With this new certification, Solar Atmospheres now operates five locations capable of fulfilling Parker Aerospace’s specific thermal processing requirements. Steve Prout, president of Solar Atmospheres’ Greenville site, highlighted the value this […]
Constellium honored with supplier of the year award from stellantis for csr excellence
Constellium, Paris, announced that it has been awarded the Supplier of the Year Award by Stellantis, recognizing the company’s strong commitment to corporate social responsibility (CSR). This honor reflects Constellium’s dedication to high CSR standards in both its operations and supply chain, which has earned positive ratings from several international rating agencies. A long-standing supplier […]
One Minute Mentor: Distortion of Ledeburitic Cold-Work Tool Steels
The different effects of steel composition on the dimensional change of plates made of ledeburitic cold-work tool steels and a working hardness of 61 HRC can be taken from the figure. Typical representatives of the new generation of improved toughness 8-9%Cr-steels show slightly higher growth in dimension than the classical 12%Cr-D2 steel. The growth in […]
Wisconsin Oven ships composite curing oven to Defense Industry
Wisconsin Oven, East Troy, WI, has announced the shipment of a gas-fired walk-in batch oven to a prominent manufacturer in the defense industry. The oven is designed for curing filament wound composite materials and is capable of processing a 78,000-pound load on a 40-foot long mandrel carried by a load car. The work chamber measures […]
Ipsen USA launches service HUB Model for improved customer support
Ipsen USA, Cherry Valley, Illinois, announced the launch of its new Service HUB model, aimed at enhancing customer support across the United States. The HUB system, developed over the past two years under the leadership of Ipsen Global CEO Geoffrey Somary and currently overseen by Chief Service Officer John Dykstra, is now fully operational across […]